Topic: Manufacturing / Casting

Which alloy is least suited for hot chamber die casting due to attack on steel components of the machine?

  • A. Tin
  • B. Lead
  • C. Aluminium
  • D. Zinc

Answer: C. Aluminium

Explanation: Aluminium is generally avoided in hot chamber die casting because molten aluminium readily attacks and dissolves the steel components (like the gooseneck and plunger) of the machine. It is cast using the cold chamber die casting process instead.