Below the ductile to brittle transition temperature, weld joints show

  • A. High ductility
  • B. High toughness
  • C. Low toughness
  • D. Ductile fracture

Answer: C. Low toughness

Explanation: Below the ductile to brittle transition temperature, materials undergo brittle fracture and weld joints show low toughness. Toughness is the area under the stress-strain curve, and for brittle materials, it is significantly lesser than for ductile materials.