A weld shows high hardness in the heat affected zone but poor impact toughness. Which change is most appropriate?

  • A. Increase cooling rate and reduce heat input
  • B. Increase heat input and reduce cooling rate
  • C. Increase electrode diameter only
  • D. Increase welding speed only

Answer: B. Increase heat input and reduce cooling rate

Explanation: High hardness combined with poor impact toughness in the Heat-Affected Zone (HAZ) typically indicates the formation of brittle microstructures like martensite, which is caused by a very rapid cooling rate. To prevent this and promote a tougher, more ductile microstructure (like pearlite or ferrite), the cooling rate should be reduced. This can be achieved by increasing the heat input or applying preheating.